Fiber-reinforced concrete incorporating locally available natural fibers in normal- and high-strength concrete and a performance analysis with steel fiber-reinforced composite concrete

期刊

JOURNAL OF COMPOSITE MATERIALS
卷 46, 期 1, 页码 111-122

出版社

SAGE PUBLICATIONS LTD
DOI: 10.1177/0021998311410492

关键词

Composite materials; natural and steel fibers; normal- and high-strength concrete; material properties

资金

  1. King Saud University, College of Engineering Research Center

向作者/读者索取更多资源

This study provides an experimental investigation on the properties of fiber-reinforced composite concrete consisting of natural fibers (coconut coir) and rounded, straight steel fibers in a comparative manner for both normal-strength concrete (NSC) and high-strength concrete (HSC). This investigation was carried out using several tests, which included workability test, compressive strength test, indirect tensile strength test, and flexural strength test. A total of 10 mix batches of NSC and HSC containing 0%, 0.5%, and 1.0% fiber volume dosage rates on coir and steel fibers were tested to determine the enhancement of mechanical properties of composite concrete. In both NSC and HSC, the workability of concrete significantly reduced as the fiber dosage rate increased. In NSC, the compressive strength test indicated that strength decreases compared to plain concrete for both types of fiber. In HSC, compressive strength decreases compared to plain concrete for coir fiber and also decreases with increasing fiber volume dosage rate and increases for steel fiber with increasing fiber volume dosage rate. In NSC, split tensile test showed that tensile strength decreased for 0.5% coir and increased for 0.5% steel compared to plain concrete. But in HSC, strength increases for 0.5% coir compared to 0.5% steel and plain concrete. In NSC, flexural strength and flexural toughness of composite concrete increased in both types of fiber. But in case of concrete with coir fiber, flexural strength for 0.5% and 1% fiber volume dosages is same and increases for steel fiber. In HSC, increase of flexural strength for 0.5% coir compared to plain concrete was observed. Flexural strength also decreases with increase of fiber volume dosage for both types of fiber. In post-cracking stage, the fibers were fully utilized when it increases the ductility and toughness of both types of concrete. This research has shown that 0.5% and 1.0% coir fibers give improved performance in flexural strength of NSC, and 0.5% coir fiber gives improved performance in flexural and tensile strengths of HSC. Also, addition of coir fibers in both types of concrete increases the ductility and toughness of concrete, whereas reduction of workability of fresh concrete and compressive strength of hardened concrete occurs using coir fibers in both types of composite concrete.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.4
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据