4.6 Article

Toughness optimization of elastomer-modified glass-fiber reinforced PA6 materials

期刊

JOURNAL OF APPLIED POLYMER SCIENCE
卷 127, 期 1, 页码 57-66

出版社

WILEY-BLACKWELL
DOI: 10.1002/app.36853

关键词

brittle-to-tough transition; glass-fibers; J-integral; PA6 elastomer blends

资金

  1. DECHEMA

向作者/读者索取更多资源

To investigate the influence of moisture and EPR-g-MA content on the fracture behavior of glassfiber reinforced PA6 materials, brittle-to-tough transition temperatures (Tbtt) were determined. Water absorption was taken into account by conditioning the analyzed materials. Tensile tests could reveal the temperature range of the largest moisture dependence of mechanical properties between 10 and 50 degrees C. J-integral values were used to describe the fracture behavior under conditions of impact load as a function of temperature. The brittle-to-tough transition of reinforced polyamides was found to be less approximate than in unreinforced materials. Two different characteristic temperature points Ts and Te were identified, which were the intercept between elastic and elasticplastic deformation on the one hand and the starting point of dominating stable crack propagation with strong plastic deformation on the other hand. Characteristic brittle-to-tough transition temperatures Tbtt could be calculated as the arithmetic average of these two points. (C) 2012 Wiley Periodicals, Inc. J. Appl. Polym. Sci., 2012

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6