Fracture behavior of thermoplastic polyolefin/clay nanocomposites

期刊

JOURNAL OF APPLIED POLYMER SCIENCE
卷 110, 期 2, 页码 864-871

出版社

JOHN WILEY & SONS INC
DOI: 10.1002/app.28560

关键词

clay; elastomers; nanocomposites; toughness

向作者/读者索取更多资源

A thermoplastic polyolefin (TPO) containing 70 wt % styrene-ethylene-butadiene-styrene-g-maleic anhydride and 30 wt % polypropylene and its nanocomposites reinforced with 0.3-1.5 wt % organoclay were prepared by melt mixing followed by injection molding. The mechanical and fracture behaviors of the TPO/clay nanocomposites were investigated. The essential work of fracture (EWF) approach was used to evaluate the tensile fracture behavior of the nanocomposites toughened with elastomer. Tensile tests showed that the stiffness and tensile strength of TPO was enhanced by the addition of low loading levels of organically modified montmorillonite. EWF measurements revealed that the fracture toughness of the TPO/clay nanocomposites increased with increasing clay content. The organoclay toughened the TPO matrix of the nanocomposites effectively. (c) 2008 Wiley Periodicals, Inc.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据