4.6 Article

Grain and the concomitant ferroelectric domain size dependent physical properties of Ba0.85Ca0.15Zr0.1Ti0.9O3 ceramics fabricated using powders derived from oxalate precursor route

期刊

JOURNAL OF APPLIED PHYSICS
卷 116, 期 16, 页码 -

出版社

AMER INST PHYSICS
DOI: 10.1063/1.4900494

关键词

-

向作者/读者索取更多资源

Fine powders comprising nanocrystallites of Ba0.85Ca0.15Zr0.1Ti0.9O3 (BCZT) were synthesized via oxalate precursor method, which facilitated to obtain homogenous and large grain sized ceramics at a lower sintering temperature. The compacted powders were sintered at various temperatures in the range of 1200 degrees C-1500 degrees C for an optimized duration of 10 h. Interestingly the one that was sintered at 1450 degrees C/10 h exhibited well resolved Morphotrophic Phase Boundary. The average grain size associated with this sample was 30 mu m accompanied by higher domain density mostly with 90 degrees twinning. These were believed to have significant contribution towards obtaining large strain of about 0.2% and piezoelectric coefficient as high as 563 pC/N. The maximum force that was generated by BCZT ceramic (having 30 mu m grain size) was found to be 161 MPa, which is much higher than that of known actuator materials such as PZT (40MPa) and NKN-5-LT (7 MPa). (C) 2014 AIP Publishing LLC.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据