Formation of an SEI on a LiMn2O4 cathode during room temperature charge-discharge cycling studied by soft X-ray absorption spectroscopy at the Fluorine K-edge

期刊

JOURNAL OF APPLIED ELECTROCHEMISTRY
卷 41, 期 11, 页码 1295-1299

出版社

SPRINGER
DOI: 10.1007/s10800-011-0344-6

关键词

LiMn2O4; SEI; LiF; Soft X-ray absorption spectroscopy; Lithium secondary batteries

资金

  1. National Research Foundation of Korea (NRF)
  2. Ministry of Education, Science, and Technology (MEST) [2010-00351]
  3. Office of Vehicle Technologies of the US Department of Energy [DE-AC02-98CH10886]
  4. National Research Laboratory through the National Research Foundation of Korea (NRF)
  5. Ministry of Education, Science and Technology (MEST) [2007-0055835]
  6. Korean Government (MKE)
  7. National Research Foundation of Korea [2011-56529, 2010-00351, 2007-0055835] Funding Source: Korea Institute of Science & Technology Information (KISTI), National Science & Technology Information Service (NTIS)

向作者/读者索取更多资源

The solid electrolyte interface (SEI) formation on the surface of LiMn2O4 electrodes during room temperature charge-discharge cycling was studied using soft X-ray absorption spectroscopy at the Fluorine (F) K-edge. LiMn2O4 electrodes without any binder were prepared by electrostatic spray deposition to eliminate the signal originating from the PVDF binder in the F K-edge X-ray absorption spectra. The F K-edge absorption spectra show that the SEI layer forms at a very early stage of cycling. SEI growth takes place during discharge. In addition, LiF formation is accelerated if the discharge step follows a charge step. The F K-edge absorption spectra suggest that the major component of the SEI is LiF.