4.7 Article

Thermal degradation of keratin waste

期刊

JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS
卷 91, 期 2, 页码 288-295

出版社

ELSEVIER SCIENCE BV
DOI: 10.1016/j.jaap.2011.03.003

关键词

Keratin; Wool; Hair; Feathers; TG-MSD/FTIR; Pyrolysis; GC-MSD

资金

  1. European Social Fund [ID POSDRU/89/1.5/S/55216]

向作者/读者索取更多资源

Thermal degradation of sheep wool, human hair and chicken feathers was studied by TG-MSD/FTIR and by pyrolysis followed by GC-MSD analysis in order to identify the degradation compounds and the temperature range in which they are formed. Only small differences were found between the studied keratin samples. They consist mainly in shift of characteristic temperatures of degradation and in relative amounts of compounds in degradation products, especially in aqueous phase. Degradation started with formation of ammonia and CO(2) (from 167 and 197 degrees C respectively and with maximum evolution at 273 and 287 degrees C respectively), continues with formation of sulphur-containing inorganic compounds (SCS, SCO, H(2)S and 502 at 240, 248, 255 and 253-260 degrees C respectively) and of water (255 C). Thiols are formed in two stages (257 and 320 C) while the evolution of nitriles is maximum around 340 C and continues up to about 480 degrees C. Phenol and 4-methylphenol are the most important degradation compounds, formed at 370 and 400 degrees C respectively. Nitrogen was present mainly in aliphatic/aromatic nitriles, pyrroles, pyridines and amides while sulphur was found mainly as sulphides, thiols, thiazoles and thiophenes. (C) 2011 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据