期刊
JOURNAL OF ALLOYS AND COMPOUNDS
卷 448, 期 1-2, 页码 308-312出版社
ELSEVIER SCIENCE SA
DOI: 10.1016/j.jallcom.2006.10.062
关键词
thermoelectric properties; (Bi,Sb)(2)Te-3; mechanical alloying; plasma activated sintering
In the present work, p-type (Bi,Sb)(2)Te-3 alloys with excess Te addition were prepared by mechanical alloying and plasma activated sintering. A preferentially orientated microstructure with the basal planes (001) perpendicular to the pressing direction was formed, and the orientation factors of the (001) planes of the Bi0.5Sb1.5Te3 and Bi0.4Sb1.6Te3 alloys were 0.12 and 0.11, respectively. Effect of excess Te content on the thermoelectric properties of the (Bi,Sb)(2)Te-3 alloys was investigated and the figure of merit of the Bi0.4Sb1.6Te3 alloys decreased from 5.26 x 10(-3) to 4.44 x 10(-3) K-1 with increasing the amount of excess Te to 8 wt.%, this should be ascribed to the fact that the chemical composition of the 8 matrix phase displayed indifference with varying excess Te content and the presence of free Te second phase. (C) 2006 Elsevier B.V. All rights reserved.
作者
我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。
推荐
暂无数据