Increasing significantly the failure strain and work of fracture of solidification processed AZ31B using nano-Al2O3 particulates

期刊

JOURNAL OF ALLOYS AND COMPOUNDS
卷 459, 期 1-2, 页码 244-250

出版社

ELSEVIER SCIENCE SA
DOI: 10.1016/j.jallcom.2007.05.038

关键词

magnesium alloy; nano-particulate; nano-composite; Al2O3

向作者/读者索取更多资源

In the present study, AZ31B magnesium alloy was unified with three different volume fractions of 50-nm Al2O3 particulates using the technique of disintegrated melt deposition. Composite samples were then subsequently hot extruded and characterized. Microstructural characterization studies revealed equiaxed grain structure, minimal porosity, reasonably uniform distribution of Al2O3 nano-particulates and good matrix-reinforcement interfacial integrity. The presence of Al2O(3) Particulates assisted in improving the thermal stability, microhardness and ductility of AZ31B alloy while 0.2%YS and UTS decreased. The overall tensile properties assessed in terms of work of fracture improved more than four times as a result of presence of 1.5 vol.% of Al2O3 nano-particulates. An attempt is made to correlate the effect of amount of Al2O3 nano-particulates on the microstructure and properties of AZ3 1B magnesium alloy. (c) 2007 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据