Glasses are known to be vulnerable to tensile stresses particularly in the presence of preexisting cracks. Since cracks in glass components are very often subjected to mixed mode loading, several researchers have studied mixed mode fracture in soda lime glass using different test specimens. Among these specimens, the cracked Brazilian disc specimen has been used most frequently by investigators. However, it is shown in this paper that the previously reported experimental results obtained from the cracked Brazilian disc specimen for several glasses are always underestimated by fracture theories like the maximum tangential stress criterion. A generalized maximum tangential stress criterion is then employed for predicting the mixed mode fracture test results. It is shown that the experimental results obtained from the cracked Brazilian disc specimen and reported in the literature for soda lime glass can be estimated very well when the generalized criterion is used. It is also shown that the same criterion can be used for predicting the test results available in the literature for brittle fracture in a glass plate containing an angled center-crack. (C) 2008 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据