期刊
INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS
卷 42, 期 -, 页码 47-50出版社
ELSEVIER SCI LTD
DOI: 10.1016/j.ijrmhm.2013.10.009
关键词
Tungsten; High pressure; Densification; Grain size; Fracture toughness
资金
- National Natural Science Foundation of China [11027405]
- China 973 Program [2011CB808200]
In this work, we present a novel method to sinter tungsten bulk material under high pressure without any additives. The sintering temperatures were greatly reduced in our experiments. The sintered samples can achieve near-full densification (relative density of 99.5%), and have fracture toughness of about 50% higher than that from the traditional methods, without sacrificing hardness. Moreover, the grain sizes of the sintered samples maintained in the initio range. The sintering kinetics, microstructure evolutions, and relationships of mechanical properties versus pressure-temperature conditions were also discussed. (C) 2013 Elsevier Ltd. All rights reserved.