Stress corrosion cracking; Welded pipe; Residual stress; S-version FEM; Surface crack

向作者/读者索取更多资源

The objective of this study is the prediction of crack propagation under thermal, residual stress fields using S-Version FEM (S-FEM). By using the S-FEM technique, only the local mesh should be re-meshed and it becomes easy to simulate crack growth. By combining with an auto-meshing technique, the local mesh is re-meshed automatically, and a curved crack path is modeled easily. Virtual crack closure integral method (VCCM) is used to evaluate energy release rate at the crack tip. For crack growth analyses, crack growth rate and growth direction are determined using criteria for mixed mode loading condition. In order to confirm the validity of this analysis, some comparisons with previously reported analyses were done, and good agreement obtained. In this study, residual stress data were provided by JAEA, Japan Atomic Energy Agency, based on their numerical simulation. Stress corrosion crack (SCC) growth analyses in a pipe are conducted in two-dimensional and three-dimensional fields. Two cases, for an axi-symmetric distribution of residual stress in the pipe wall and a non-axisymmetric one are assumed. Effects of residual stress distribution patterns on SCC cracking are evaluated and discussed. (C) 2011 Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.5
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据