4.7 Article

Impact of cross-linker on alginate matrix integrity and drug release

期刊

INTERNATIONAL JOURNAL OF PHARMACEUTICS
卷 355, 期 1-2, 页码 259-268

出版社

ELSEVIER
DOI: 10.1016/j.ijpharm.2007.12.038

关键词

lamination; cross-linking; disintegration; barrier preservation; modified release

向作者/读者索取更多资源

Sodium alginate, a biopolymer, was employed in the formulation of matrix tablets. They cracked or laminated at acidic pH, compromising their dissolution performance. Improved mechanical strength and reduced barrier permeability of calcium alginate gel provided the rationale for cross-linking the alginate matrix to sustain drug release. Studies had suggested that the incorporation of soluble calcium salts in alginate matrix tablets could sustain drug release at near-neutral pH due to in situ cross-linking. However, results from the present study showed otherwise when gastrointestinal pH conditions were simulated. Significant reduction in drug release rate was only observed when an external calcium source was utilized at low concentration. High calcium ion concentrations caused matrix disintegration. In contrast, matrices pre-coated by calcium alginate could sustain drug release at pH 1.2 followed by pH 6.8 for over 12 h. The presence of cross-linked barrier impeded matrix lamination and preserved matrix structure, contributing to at least three-fold reduction in drug release at pH 1.2. Zero order release as well as delayed burst release could be achieved by employing appropriate grade of alginate and cross-linking conditions. (C) 2008 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据