4.7 Article

Experimental investigation of pinhole effect on MEA/cell aging in PEMFC

期刊

INTERNATIONAL JOURNAL OF HYDROGEN ENERGY
卷 38, 期 1, 页码 543-550

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.ijhydene.2012.09.058

关键词

Electrochemical surface area; H-2 crossover; Impedance spectroscopy; MEA aging; PEM fuel cell; Pinhole effect

资金

  1. French National Research Agency (ANR) within the DamaS project [ANR 08-JCJC-0052-01]
  2. Agence Nationale de la Recherche (ANR) [ANR-08-JCJC-0052] Funding Source: Agence Nationale de la Recherche (ANR)

向作者/读者索取更多资源

The effect of MEA pinhole size on the aging of single (10 x 10 cm(2)) PEMFC was investigated. Two MEAs were perforated by two pins of different diameters (0.7 and 1.2 mm), in both cases in the H-2 inlet zone. The performance losses and the degradation rates of the MEA components were compared to those exhibited by a healthy, not perforated MEA. Perforation by the smaller pin did not promote immediate cell voltage decay and the hydrogen crossover increased only slightly. Perforation by the larger pin resulted in immediate reduction in cell voltage and one decade increase of the hydrogen crossover. LSV and CV voltammograms performed for determination of the crossover and the electrode active surface were changed abruptly by the larger perforation, which confirmed the existence of an internal short circuit within the MEA. Besides, the perforation affected the time variations of the diffusion and charge transfer resistances. Copyright (C) 2012, Hydrogen Energy Publications, LLC. Published by Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据