Thermal cycling and ageing of a glass-ceramic sealant for planar SOFCs

期刊

INTERNATIONAL JOURNAL OF HYDROGEN ENERGY
卷 36, 期 18, 页码 11895-11903

出版社

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.ijhydene.2011.04.083

关键词

Glass-ceramic sealant; Solid oxide fuel cell; Trasmission electron microscopy; Microstructure; Crofer22APU

向作者/读者索取更多资源

Thermal cycling and thermal ageing tests were performed on Crofer22APU/glass-ceramic/Anode-Supported-Electrolyte (ASE) joined samples in air at the SOFC operating temperature of 800 degrees C. The Crofer22APU had been polished and preoxidised at 900 degrees C for 2 h. The diffusion behaviour at the two interfaces was examined and revealed slight diffusion of chromium and manganese from Crofer22APU into the glass-ceramic. No interactions, failure or crack formation were observed at the Crofer22APU/glass-ceramic interface and between the glass-ceramic and YSZ. Copyright (C) 2011, Hydrogen Energy Publications, LLC. Published by Elsevier Ltd. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据