4.6 Article

A comparison of the tensile, fatigue, and fracture behavior of Ti-6Al-4V and 15-5 PH stainless steel parts made by selective laser melting

期刊

出版社

SPRINGER LONDON LTD
DOI: 10.1007/s00170-013-5106-7

关键词

Fatigue; Fracture; Fractography; Additive manufacturing; Selective laser melting; Ti-6Al-4V; 15-5 PH steel; Direct metal laser sintering

资金

  1. Office of Naval Research (ONR), USA [N00014-09-1-0147]

向作者/读者索取更多资源

In this work, Ti-6Al-4V and 15-5 PH steel samples were fabricated using selective laser melting (SLM) and their tensile, fatigue, and fracture properties were analyzed and compared. The tensile properties were compared with respect to the build orientation. The horizontally built samples showed relatively better tensile properties as compared with the vertically built samples. Fatigue performance was studied for the vertical build orientation and compared with standard wrought material data. The tensile and fatigue performance of SLM-built materials were comparable to their respective standard wrought materials. Fractography was carried out for all tensile and fatigue-tested samples. The fatigue fracture behavior of Ti-6Al-4V was different from 15-5 PH steel. For Ti-6Al-4V, the fatigue crack initiation occurred deep in the subsurface whereas for PH steel the fatigue crack was initiated from the surface.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.6
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据