Synthesis and electrical conductivity of crystalline and glassy alloys in the Ag3GeS3Br-GeS2 system

期刊

INORGANIC MATERIALS
卷 49, 期 9, 页码 867-871

出版社

MAIK NAUKA/INTERPERIODICA/SPRINGER
DOI: 10.1134/S0020168513090100

关键词

-

向作者/读者索取更多资源

We have studied the formation of crystalline and glassy alloys in the Ag3GeS3Br-GeS2 system (0-52 mol % GeS2; Ag3GeS3Br is a glass-forming phase of variable composition) and determined the crystallographic parameters of the Ag3.179(9)Ge1.474(5)S4Br alloy as the saturated solid solution of GeS2 in Ag3GeS3Br: sp. gr. P2(1)3, a = 10.16572(3) , Z = 4. The electrical conductivity of the crystalline and glassy alloys was measured in the temperature range 250-410 K by a dc probe technique. The current carriers in the alloys are silver cations and halogen anions. We obtained materials with superionic conductivity and proposed a model for conduction in the alloys.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.2
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据