Alumina borate whiskers with a SnO2 Bi2O3 coating reinforced pure aluminum composite was fabricated by squeeze casting. The damping behavior of the composite, which had undergone thermal cycling during the internal friction measurement, was described. It was found that there is one internal friction peak in the heating process, but there are three internal friction peaks in the cooling process. The formation of Bi-Sn eutectic at the whisker/Al interface in the composite, after having undergone one thermal cycle, is the main factor affecting the behavior and mechanism of the internal friction of the composite before and after having undergone thermal cycling. (C) 2014 Elsevier B.V. All rights reserved.

作者

我是这篇论文的作者
点击您的名字以认领此论文并将其添加到您的个人资料中。

评论

主要评分

4.7
评分不足

次要评分

新颖性
-
重要性
-
科学严谨性
-
评价这篇论文

推荐

暂无数据
暂无数据