Electrochemistry and in situ Raman spectroelectrochemistry of low and high quality boron doped diamond layers in aqueous electrolyte solution

Journal

ELECTROCHIMICA ACTA
Volume 87, Issue -, Pages 518-525

Publisher

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.electacta.2012.09.031

Keywords

Boron doped diamond; Electrochemistry; Aqueous electrolyte solution; Raman spectroscopy; In situ Raman spectroelectrochemistry

Funding

  1. FP7-Energy-2010-FET Project Molesol [256617]
  2. Academy of Sciences of the Czech Republic [IAA 400400804, KAN 200100801]

Ask authors/readers for more resources

In this work we report on electrochemical and in situ Raman spectroelectrochemical characterization of low quality (LQ) ultrathin nanocrystalline and high quality (HQ) polycrystalline boron doped diamond (BDD) compared especially in terms of the sp(2) carbon content. The BDD films were grown by microwave plasma enhanced chemical vapor deposition and doped with various boron concentrations from 250 to 8000 ppm (boron/carbon ratio in the gas phase) at different conditions. The quality (presence of graphitic or amorphous phases) and boron doping levels in the BDD films were analyzed by micro-Raman spectroscopy. From the neutron depth profiling, it was found that the boron content in the near surface region (<1 mu m) was in the range from about 4 x 10(19) cm(-3) to 58 x 10(20) cm(-3) for B/C from 250 ppm to 8000 ppm, respectively. The electrochemical measurements have been performed in aqueous 0.5 M H2SO4 in the potential range from 2 to 2.5 V vs. Hg/Hg2SO4. Cyclic voltammetry showed that the electrochemical potential window was independent on the boron doping but depended on the film quality, i.e. when the sp(2) carbon content increased the width of potential window decreased. The in situ Raman spectroelectrochemistry was performed in aqueous electrolyte solution (0.5 M H2SO4) in the potential range from 1.5 to 1.5 V vs. Hg/Hg2SO4 using two laser excitations (633 nm and 457 nm). In the case of films containing high amount of sp(2) carbonaceous phase (low quality), the modes belonging to sp(2) carbonaceous phases changed their intensities. The intensity of the D, G and D' Raman peaks increased in cathodic direction, while in anodic direction bleaching of these peaks was observed. The diamond films prepared with very small amount of sp(2) carbon (high quality) exhibited no spectroelectrochemical changes in the potential region tested. (C) 2012 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.6
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available