Tribocorrosion behaviour of aluminium bronze in 3.5 wt.% NaCl solution

Journal

CORROSION SCIENCE
Volume 144, Issue -, Pages 207-223

Publisher

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.corsci.2018.08.058

Keywords

Tribocorrosion; Plastic deformation; Selective dissolution; Wear; Corrosion

Funding

  1. SUBTRIB project from the Finnish Funding Agency for Technology and Innovation (Tekes) [865/31/2016]
  2. VTT Technical Research Centre of Finland Ltd

Ask authors/readers for more resources

Tribocorrosion behaviour of aluminium bronze CuAl10Fe5Ni5 in 3.5 wt.% NaCl solution was investigated in a pin-on-disc facility containing an electrochemical cell. Oxidising capacity and contact pressure to alumina counterbody were varied. Pure corrosion occurred as selective dissolution of a phase included in the eutectoid structure. Contact to counterbody introduced plastic deformation, extrusion of the material and abrasive wear. Wear-corrosion interactions varied between the two contact pressures, with lower material losses appearing at the higher pressure. The significant acceleration of material degradation by the interactions was not clearly reflected to kinetics or thermodynamics of corrosion. These results are presented and discussed here.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available