PEDOT films were deposited by microwave (MW) and radio frequency (RF) plasma in a medium pressure of 0.02 Torr without precursor. In-situ optical emission spectroscopy (OES) measurement was carried out to determine plasma phase and to adjust discharge parameters. The other spectroscopic methods were used to characterize deposited thin films and to compare the effect of discharge parameters on the process. Conductivity values were found to be around up to 10(-5) S/cm for MW plasma, and 10(-8) S/cm for RF plasma deposited PEDOT films, without the addition of a doping agent. It was found that both plasma polymerization methods resulted in crosslinked PEDOT structures.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.3
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available