4.7 Article

The fate of sulfur during rapid pyrolysis of scrap tires

Journal

CHEMOSPHERE
Volume 97, Issue -, Pages 102-107

Publisher

PERGAMON-ELSEVIER SCIENCE LTD
DOI: 10.1016/j.chemosphere.2013.10.037

Keywords

Scrap tires; Rapid pyrolysis; Sulfur; Speciation

Funding

  1. National Natural Science Foundation of China [51076053, 51161140330]
  2. Key Project of Chinese National Programs for Fundamental Research and Development (973 program) [2011CB201505]

Ask authors/readers for more resources

The fate of sulfur during rapid pyrolysis of scrap tires at temperatures from 673 to 1073 K was investigated. Sulfur was predominant in the forms of thiophenic and inorganic sulfides in raw scrap tires. In the pyrolysis process, sulfur in organic forms was unstable and decomposed, leading to the sulfur release into tar and gases. At 673 and 773 K, a considerable amount of sulfur was distributed in tar. Temperature increasing from 773 to 973 K promoted tar decomposition and facilitated sulfur release into gases. At 1073 K, the interactions between volatiles and char stimulated the formation of high-molecular-weight sulfur-containing compounds. After pyrolysis, almost half of the total content of sulfur in raw scrap tires still remained in the char and was mostly in the form of sulfides. Moreover, at temperatures higher than 873 K, part of sulfur in the char was immobilized in the sulfates. In the pyrolysis gases, H2S was the main sulfur-containing gas. Increasing temperature stimulated the decomposition of organic polymers in scrap tires and more H2S was formed. Besides H2S, other sulfur-containing gases such as CH3SH, COS and SO2 were produced during the rapid pyrolysis of scrap tires. (C) 2013 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available