4.7 Article

Mesoporous MgO sorbent promoted with KNO3 for CO2 capture at intermediate temperatures

Journal

CHEMICAL ENGINEERING JOURNAL
Volume 258, Issue -, Pages 254-264

Publisher

ELSEVIER SCIENCE SA
DOI: 10.1016/j.cej.2014.07.088

Keywords

CO2 capture; Intermediate temperature; MgO composite; Aerogel; KNO3

Funding

  1. Korea CCS RD Center
  2. Ministry of Education, Science and Technology
  3. Korea Institute of Energy Technology Evaluation and Planning [20118510020030-12-1-000]
  4. Ministry of Trade, Industry Energy
  5. Korea Evaluation Institute of Industrial Technology (KEIT) [20118510020030] Funding Source: Korea Institute of Science & Technology Information (KISTI), National Science & Technology Information Service (NTIS)
  6. National Research Foundation of Korea [2012-0008929] Funding Source: Korea Institute of Science & Technology Information (KISTI), National Science & Technology Information Service (NTIS)

Ask authors/readers for more resources

Mesoporous MgO center dot KNO3 composites were developed using an aerogel method for CO2 sorption in the intermediate temperature range of 250-400 degrees C. The effects of MgO/KNO3 molar ratio, calcination method and sorption temperature on CO2 sorption rate and capacity were evaluated using a thermogravimetric analyzer. The composite prepared at a MgO/KNO3 molar ratio of 1:0.2 with a four-step calcination had the high CO2 sorption capacity of 13.9 wt% at 325 degrees C and 120 min, showing about 70% of the total sorption capacity within 10 min and about 7 times higher sorption capacity than pure MgO. In addition, the developed MgO center dot KNO3 composite showed higher sorption capacity than other MgO composites promoted by alkali metal salts (K2CO3, KOH, NaNO3, Na2CO3, Na2HPO4, LiNO3 and Li2CO3). The sorption rate of CO2 on a MgO center dot KNO3 composite during the initial 30 min was on the order of 10(-4)/s. Sorption working capacity was evaluated by 12 cyclic tests at 325 and 375 degrees C for sorption (20 min) and 450 degrees C for regeneration (30 min). Sorption working capacity was higher at 325 degrees C than at 375 degrees C, but MgO/KNO3 was highly stable at 375 degrees C, showing 90 wt% of the first cycle. (C) 2014 Elsevier B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available