Effect of drying method on mesoporosity of resorcinol-formaldehyde drygel and carbon gel

Journal

DRYING TECHNOLOGY
Volume 19, Issue 7, Pages 1319-1333

Publisher

MARCEL DEKKER INC
DOI: 10.1081/DRT-100105291

Keywords

BET surface area; freeze drying; hot air drying; microwave drying; pore size distribution; pyrolysis; sol-gel polycondensation

Ask authors/readers for more resources

Resorcinol-formaldehyde hydrogels were synthesized by sol-gel polycondensation of resorcinol with formaldehyde in a slightly basic aqueous solution. RF cryogels, RF xerogels, and RF xerogels (MW gets) were respectively prepared from RF hydrogels by freeze drying, hot air drying, and microwave drying. Carbon cryogels, carbon xerogels and carbon MW gels were subsequently obtained by pyrolyzing RF drygels in an inert atmosphere. Freeze drying and microwave drying were effective to prepare mesoporous RF drygels and carbon gels. RF cryogels and carbon cryogels showed high mesoporosity over wide ranges of the molar ratio of resorcinol to catalyst (R/C) and the ratio of resorcinol to water (R/W) used in sol-gel polycondensation, Although RF xerogels had a few mesopores, carbon xerogels had no mesopores. RF MW gels and carbon MW gels showed mesoporosity if appropriate values of R/C and R/W were selected.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.5
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available