Tungsten oxide (WO3) films prepared by annealing electrochemically anodized metallic tungsten (W) films deposited by radio-frequency sputtering were characterized. Tungsten oxide films of various morphology, crystallinity, and porosity can be prepared by carefully altering the anodization time (20-50 min) and annealing temperature (450-550 degrees C). The film obtained after 40 min of anodization, and that annealed at 500 degrees C shows the best electrochromic performance with optical modulation of 43.6% and coloration efficiency of 42.8 cm(2)/C. The effects of anodization time and annealing temperature on microstructure and electrochromic properties were addressed. (C) 2012 Elsevier Ltd and Techna Group S.r.l. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available