4.3 Article

Sonochemical synthesis of tungsten sulfide nanorods

Journal

JOURNAL OF MATERIALS CHEMISTRY
Volume 12, Issue 5, Pages 1450-1452

Publisher

ROYAL SOC CHEMISTRY
DOI: 10.1039/b110867k

Keywords

-

Ask authors/readers for more resources

Amorphous WS2 has been prepared by ultrasound irradiation of W(CO)(6) solution in diphenylmethane (DPhM) in the presence of a slight excess of sulfur at 90 degreesC under argon. Heating the amorphous powder at 800 degreesC under argon yields WS2 nanorods and their packings. The average size of WS2 nanorods was found to be 3-10 nm and 1-5 mum in thickness and length, respectively. The prepared WS2 has been characterized by elemental analysis, X-ray powder diffraction measurements, FTIR spectroscopy, differential scanning calorimetry, thermogravimetric analysis, transmission electron microscopy, scanning electron microscopy, atomic force microscopy and energy dispersive X-ray analysis.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.3
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available