The reduction of FeO from iron-saturated FeO-CaO-Al2O3-SiO2 slags by graphite, coke and coal char at 1 673 K has been investigated using a sessile drop technique. Metallographic analysis of samples quenched from the reaction temperature, and in situ observations of the reaction interface, reveal significant differences in the slag/carbon contact, and in the morphologies of the product iron and its composition; these differences were found to depend on the carbon type used in the reduction. In particular it has been shown that, in the case of graphite and coke, liquid Fe-C droplets were rapidly formed at the slag/C interface. Reactions of the slag with coal chars, in contrast, result predominantly in the formation of solid iron. These observations indicate that the reaction pathways, and hence reaction kinetics, are dependent on carbon type.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.4
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available