An investigation was made into the Bi(Mg0.75W0.25)O-3-PbTiO3 (BMW-PT) system. The aim was to find the optimum composition with respect to piezoelectric and dielectric properties and link this to the presence of a morphotropic phase boundary (MPB). The optimum composition was found to be 62 mol% PT. The maximum values of the piezoelectric constant d(33) = 150 pm/V and the maximum relative dielectric constant epsilon(33)/epsilon(0) = 1400. The dielectric loss is high with tan 6 typically similar to 5%. Results from capacity versus the temperature measurements indicate a Curie temperature of 220 degrees C, which is significantly lower than the predicted value. (c) 2004 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available