4.7 Article

High strength and bioactive hydroxyapatite nano-particles reinforced ultrahigh molecular weight polyethylene

Journal

COMPOSITES PART B-ENGINEERING
Volume 38, Issue 3, Pages 345-351

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.compositesb.2006.05.004

Keywords

nano-structures; directional orientation; mechanical properties; extrusion

Ask authors/readers for more resources

Nano-sized hydroxyapatite (HA) particles reinforced UHMWPE composite was developed for biomedical applications. The biocomposite with HA volume fraction of 0.5 was successfully processed by combined swelling/twin-screw extrusion, compression molding, and then hot drawing. SEM and EDAX characterization revealed that HA nano-particles were homogeneously dispersed in UHMWPE. WAXD showed that hot drawing effectively oriented the UHMWPE chains along the drawing direction. The composite exhibited tensile strength of 100 +/- 22 MPa after hot drawing, which was comparable to that of cortical bone. The composite also exhibited great ability of inducing calcium phosphate precipitates on its surface in simulated body fluid, which was widely accepted as an indication of bioactivity. (c) 2006 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available