This study aims at the interpretation of the adverse effects of the secondary products in two types of rocks during their performance as concrete aggregates. Serpentinised peridotites contain serpentine, as the dominant secondary phase, which creates low microroughness on the particles and therefore unfavorable surfaces for cement paste to adequately adhere to. Moreover, its soft and platy nature contributes to the development of platy defects along the contacts of the aggregate particles with the cement paste. Poor adherence of the paste, failures along the contacts of the aggregate particles and potential propagation of the defects into the concrete during curing (and perhaps subsequently in-service) explain the poor performance of highly serpentinised rocks as concrete aggregates. Andesites show a different composition with a variety of secondary products including albite, chlorite, calcite, Fe-oxides and clay minerals. The role of all these products was investigated and it appears that only smectite is important, as even small amounts of it may be detrimental to the quality of the rocks as concrete aggregates. It is likely that abnormal hydration reactions and considerable swelling of the smectite result in the appearance of defects in the concrete, hence contributing to its low performance.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.1
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available