4.8 Article

Cr and Ni recovery during bioleaching of dewatered metal-plating sludge using Acidithiobacillus ferrooxidans

Journal

BIORESOURCE TECHNOLOGY
Volume 167, Issue -, Pages 61-68

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.biortech.2014.05.107

Keywords

Bioleaching; Dewatered metal-plating sludge; Acidithiobacillus ferrooxidans; Kinetics; Optimization

Funding

  1. Iran National Science Foundation (INSF) [91058087]

Ask authors/readers for more resources

This study determined the optimal conditions required to attain maximum metal recovery in the bioleaching process of dewatered metal-plating sludge using Acidithiobacillus ferrooxidans (A. ferrooxidans). Adaptation of this strain was carried up to 1% (w/v) of the sample. Three factors including initial pH, initial Fe3+ concentration and pulp density were selected as the effective factors and were optimized using a central composite design of response surface methodology. An initial pH of 1, pulp density of 9 g/l and initial Fe3+ concentration of 1 g/l were determined to be optimum values by the statistical models. The highest extractions for Cr and Ni under optimal conditions were 55.6% and 58.2%, respectively. Bioleaching kinetics was investigated using a modified shrinking core model to better understand the mechanism of the leaching reaction. The model predictions indicate that the diffusion step controlled the overall dissolution kinetics and is the rate controlling step. (C) 2014 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.8
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available