4.7 Article

Preparation of chitin nanofibers from squid pen β-chitin by simple mechanical treatment under acid conditions

Journal

BIOMACROMOLECULES
Volume 9, Issue 7, Pages 1919-1923

Publisher

AMER CHEMICAL SOC
DOI: 10.1021/bm800178b

Keywords

-

Ask authors/readers for more resources

A procedure for preparing individualized chitin nanofibers 3-4 nm in cross-sectional width and at least a few microns in length was developed. The key factors to prepare the chitin nanofibers with such high aspect ratios are as follows: (1) squid pen beta-chitin is used as the starting material and (2) ultrasonication of the beta-chitin in water at pH 3-4 and 0.1-0.3% consistency for a few minutes. Transparent and highly viscous dispersions of squid pen beta-chitin nanofibers in water can be obtained by this method. No N-deacetylation occurs on the chitin molecules during the nanofiber conversion procedure. Moreover, the original crystal structure of beta-chitin is maintained, although crystallinity index decreases from 0.51 to 0.37 as a result of the nanofiber conversion. Cationization of the C2 amino groups present on the crystallite surfaces of the squid pen beta-chitin under acid conditions is necessary for preparing the nanofibers.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available