4.8 Article

Optimization of monosaccharide recovery by post-hydrolysis of the water-soluble hemicellulose component after steam explosion of softwood chips

Journal

BIORESOURCE TECHNOLOGY
Volume 72, Issue 3, Pages 207-211

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/S0960-8524(99)00125-X

Keywords

hemicelluloses; steam explosion; fermentation; softwood

Ask authors/readers for more resources

SO2-catalyzed steam explosion effectively fractionates softwood carbohydrates, releasing 80-90% of the hemicellulose into solution and enhancing the enzymatic hydrolysis of the water-insoluble cellulose fraction. When steam pretreatment conditions were modified to ensure maximum hemicellulose recovery, a significant Dart of hemicellulose-derived carbohydrates were solubilized in an oligomeric form that was not readily fermented. When Douglas fir wood chips were used as the substrate, sulfuric acid-catalyzed post-hydrolysis at 120 degrees C for 1 h allowed most of the original hemicellulose to be recovered in the monomeric form. Although higher catalyst concentrations (1-3%) resulted in complete depolymerization of the carbohydrates, noticeable losses due to sugar degradation were observed. Lower concentrations of the added catalyst increased the monomer yields, and resulted in less secondary degradation. Partial oxidation of the added SO2 to sulfuric acid during steam explosion resulted in the depolymerization of the hemicelluloses during post-hydrolysis, even without further acid addition. Hexoses present in the post-hydrolyzates could be readily fermented to ethanol. (C) 1999 Elsevier Science Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.8
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available