Dual modes of degradation by Fistulina hepatica in xylem cell walls of Quercus robur

Journal

MYCOLOGICAL RESEARCH
Volume 104, Issue -, Pages 846-852

Publisher

ELSEVIER SCI LTD
DOI: 10.1017/S0953756299002063

Keywords

-

Categories

Ask authors/readers for more resources

Sequential effects of colonisation by the wood decaying Fistulina hepatica were examined microscopically in naturally infected and artificially inoculated heartwood of pedunculate oak (Quercus robur). For 6 mo, the deposition of brown materials within parenchyma cells containing hyphae was the only visible effect of colonisation. After 12 mo degradation occurred but was initially confined to parenchyma of xylem rays, in which the secondary cell walls showed helically orientated internal cavities containing hyphae, as in a soft rot. The hyphae were covered with a resinous material and persisted in a herring bone pattern after the secondary walls became heavily degraded. The adjacent libriform wood fibres also showed cavity formation. By contrast fibre-tracheids were mainly affected by a brown rot. uv-microscopy indicated that cell types in which the soft rot mode occurred were rich in syringyl lignin, whereas the brown rot was associated with cells rich in guaiacyl lignin. Thus, the present study shows that F. hepatica possesses dual modes of degradation which appear to correlate with the different lignin composition within cell types of oak.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

3.8
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available