4.4 Article

Cathodic film formation during chromium electrolysis on low-carbon steel using short duration current steps

Journal

JOURNAL OF APPLIED ELECTROCHEMISTRY
Volume 31, Issue 5, Pages 531-536

Publisher

KLUWER ACADEMIC PUBL
DOI: 10.1023/A:1017581608574

Keywords

anodic dissolution; cathodic film; chromium plating; continuous coating line; tin-free steel

Ask authors/readers for more resources

Short duration galvanostatic electrolyses of chromium plating solutions (1.0 M CrO3 and 0.01 M H2SO4) were performed on rotating disk electrode of low-carbon steel. The influence of sulphate concentration (0.01 and 0.02 M), cathodic current density (30, 60 and 90 A dm(-2)), temperature (25, 40 and 55 degreesC), electrode rotation rate (25 to 1000 rpm) and Na2SiF6 addition (0.01 M) on E/t curves and cathodic current efficiency was investigated. Electrical charge was always consumed to form a cathodic film and effective metallic chromium deposition only occurred when the potential reached a low and stable value. The determination of cathodic current efficiency after short duration electrolyses corroborated these results. The time required to form the cathodic film decreased with current density and addition of Na2SiF6 and increased with sulphate concentration, temperature and electrode rotation rate, suggesting that this film is not completely compact. A passive film is formed at the onset of the electrolysis process and a viscous layer is formed on the surface of the first film.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.4
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available