(Ti,Al,Si)N films have been prepared by d.c. and rf reactive magnetron sputtering, with Si contents in the range 2-11 at.% and Al contents between 4 and 19 at.%. Samples prepared in rotation mode (three magnetrons) presented densities between 4.0 and 4.6 g/cm(3), while samples prepared in static mode (magnetron with Ti target with small pieces of Si and Al) displayed densities mainly in the range 3.0-3.9 g/cm(3). For comparison purposes, the evaluation of Young's modulus was performed by both depth-sensing indentation and surface acoustic wave (SAW) techniques. Indentation results revealed systematically higher values than those obtained by SAW. These discrepancies might be related with the relatively low density of the films. Hardness values of approximately 60 GPa were obtained with samples with a composition of approximately 28.5 at.% titanium, 12 at.% aluminium, 9.5 at.% silicon and 50 at.% nitrogen. XRD patterns showed the presence of two different crystalline phases, as in the case of (Ti,Si)N films. One is assigned to TiN phase (lattice parameter of approx. 0.429 nm) and the second, the so-called solid solution which is developed in situations of low surface mobility, revealed a lattice parameter (0.419 nm) slightly lower than that of bulk TiN. (C) 2001 Elsevier Science B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available