4.8 Article

Effect of oxygen delignification on the rate and extent of enzymatic hydrolysis of lignocellulosic material

Journal

BIORESOURCE TECHNOLOGY
Volume 79, Issue 2, Pages 113-120

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/S0960-8524(01)00055-4

Keywords

-

Ask authors/readers for more resources

In this study, we examined the effect of oxygen delignification on the rate and extent of enzymatic hydrolysis (using commercial cellulase and P-glucosidase) of a number of lignocellulosic substrates, including kraft pulp (model substrate), pulp mill primary clarifier sludge (PCS) and steam-exploded Douglas fir chips. Oxygen delignification removed up to 67% of the lignin from softwood pulp and improved the rate of, and yield from, hydrolysis by up to 111% and 174%, respectively. Glucose yield varied linearly with fractional lignin removal. Oxygen delignification of primary clarifier sludge improved hydrolysis yield by up to 90%. However steam-exploded Douglas fir was very resistant to hydrolysis at low enzyme loading, and oxygen delignification decreased hydrolysis rate and yield. (C) 2001 Elsevier Science Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.8
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available