Background: This study evaluated mechanical properties of glass ionomer cements (GICs) used for atraumatic restorative treatment. Wear resistance, Knoop hardness (Kh), flexural (F-s) and compressive strength (C-s) were evaluated. The GICs used were Riva Self Cure (RVA), Fuji IX (FIX), Hi Dense (HD), Vitro Molar (VM), Maxxion R (MXR) and Ketac Molar Easymix (KME). Methods: Wear was evaluated after 1, 4, 63 and 365 days. Two-way ANOVA and Tukey post hoc tests (P = 0.05) analysed differences in wear of the GICs and the time effect. F-s, C-s, and Kh were analysed with one-way ANOVA. Results: The type of cement (p < 0.001) and the time (p < 0.001) had a significant effect on wear. In early-term wear and Kh, KME and FIX presented the best performance. In long-term wear, F-s and C-s, KME, FIX and HD had the best performance. Strong explanatory power between F-s and the Kh (r(2) = 0.85), C-s and the Kh (r(2) = 0.82), long-term wear and F-s of 24 h (r(2) = 0.79) were observed. Conclusions: The data suggested that KME and FIX presented the best in vitro performance. HD showed good results except for early-term wear.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.1
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available