Defect chemistry and physical properties of transparent conducting oxides in the CdO-In2O3-SnO2 system

Journal

THIN SOLID FILMS
Volume 411, Issue 1, Pages 106-114

Publisher

ELSEVIER SCIENCE SA
DOI: 10.1016/S0040-6090(02)00197-9

Keywords

transparent conducting oxides; phase diagram; point defects; electrical properties; optical properties

Ask authors/readers for more resources

Combined solid state phase diagram studies and physical property measurements of the various n-type transparent conducting oxide (TCO) phases in the CdO-In2O3-SnO2 system have been carried out. The 1175 degreesC (air) subsolidus phase diagram has been established, including solid solution limits for binary and ternary compositions. From these limits and electrical property measurements vs. doping and degree of reduction, the prevailing defect mechanisms can be deduced. In addition to intrinsic (native) defects (e.g. oxygen vacancies) and extrinsic donor-doping of the end member compounds (e.g. Sn-In(circle) in In2O3) ternary solid solutions exhibit both isovalent doping (e.g. [Cd'(In)] = [Sn-In(circle)] in bixbyite, spinel) and donor-to-acceptor imbalance (e.g. [Sn-In(circle)] > [Cd'(In)] in bixbyite, spinel). Aliovalent doping can also lead to the formation of point defect associates, as in Sn-doped In2O3 (ITO), as confirmed by combined Rietveld analyses of X-ray and neutron diffraction data. Cation exchange between sublattices in the spinel phase plays an important role in determining phase stability and band structure. The physical properties of the TCO phases in the CdO-In2O3-SnO2 system are presented for both bulk ceramics and thin films. (C) 2002 Elsevier Science B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.4
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available