Zinc oxide nanostructures by chemical vapour deposition as anodes for Li-ion batteries

Journal

JOURNAL OF ALLOYS AND COMPOUNDS
Volume 640, Issue -, Pages 321-326

Publisher

ELSEVIER SCIENCE SA
DOI: 10.1016/j.jallcom.2015.03.222

Keywords

Zinc oxide; Chemical vapour deposition; Nanostructure; Thin film; Lithium battery

Ask authors/readers for more resources

ZnO nanostructures are grown by a simple chemical vapour deposition method directly on a stainless steel disc current collector and successfully tested in lithium cells. The structural/morphological characterization points out the presence of well-defined polycrystalline nanostructures having different shapes and a preferential orientation along the c-axis direction. In addition, the high active surface of the ZnO nanostructures, which accounts for a large electrode/electrolyte contact area, and the complete wetting with the electrolyte solution are considered to be responsible for the good electrical transport properties and the adequate electrochemical behaviour, as confirmed by cyclic voltammetry and galvanostatic charge/discharge cycling. Indeed, despite no binder or conducting additives are used, when galvanostatically tested in lithium cells, after an initial decay, the ZnO nanostructures can provide a rather stable specific capacity approaching 70 mu A h cm(-2) (i.e., around 400 mA h g(-1)) after prolonged cycling at 1 C, with very high Coulombic efficiency and an overall capacity retention exceeding 62%. (C) 2015 Elsevier B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available