Polymeric phosphonate esters are an interesting class of organophosphorus polymers because both the polymer backbone and phosphorus substituents can be modified. These polymers have been prepared by ring-opening polymerizations of cyclic phosphites, stoichiometric polycondensations of dimethyl phosphonate with diols in conjunction with diazomethane treatment and by transesterification of polyphosphonate oligomers. Our initial attempts to prepare high molecular weight polymeric phosphonate esters by the transesterification methods were unsuccessful. Results indicate that the reactions of dimethyl phosphonate with diols to form polyphosphonate oligomers with only methyl phosphonate end groups are plagued by a serious side reaction that forms phosphonic acid end groups. These end groups do not participate in the transesterification reaction and limit the molecular weights of the polymers that can be obtained. The phosphonic acid end groups can be converted into reactive methyl phosphonate end groups by treatment with diazomethane, however diazomethane is explosive and the polymerization is slow. An alternative route for the production of high molecular weight polymers is the transesterification of the 1,12-bis(methyl phosphonato)dodecane, formed by the reaction of excess dimethyl phosphonate and 1,12-dodecanediol, with a Na2CO3 promoter. This allows polymers with molecular weights of up to 4.5 x 10(4) to be prepared, and no phosphonic acid end groups are observed in these polymers. Thermal analyses of the poly(1,12-dodecamethylene phosphonate) have shown that this polymer has reasonable thermal stability (onset of thermal decomposition at 273 degreesC). This polymer also undergoes a cold crystallization process at 15degreesC similar to that which has been observed in some polyesters, polyamides and elastomers. (C) 2003 Elsevier Science Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available