The melting behaviour of poly(vinylidene fluoride) (PVDF) was investigated by differential scanning calorimetry (DSC) and small- and wide-angle X-ray scattering in order to study the influence of the chain defects content and of the temperature of annealing on the crystallization and melting behaviour. All the DSC scans show a double endotherm and the analysis of the data suggests that the low temperature endotherm is due to the melting of a population of thin lamellae, whose thickness increases during the annealing, but a high content of chain defects prevents the lamellar thickening and the main effect in this case is the crystallization of thin lamellae from a portion of polymer which did not crystallize during the quenching from the melt. Furthermore, the two melting endotherms, which are observed, can be partially ascribed to a melting-recrystallization process. Furthermore, stepwise isothermal cooling was performed in a differential scanning calorimeter followed by melting scans of fractionated PVDF samples to point out the possible presence of a series of endothermic peaks. (C) 2003 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available