The glass transition and interfacial layer in styrene-butadiene rubber containing silica nanofiller

Journal

POLYMER
Volume 44, Issue 20, Pages 6259-6266

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/S0032-3861(03)00667-0

Keywords

nanofiller; composite; mechanical relaxation

Ask authors/readers for more resources

The mechanical behaviour of a styrene-butadiene rubber, containing 23.5% styrene and filled with up to 55% by weight with silica nanoparticles, has been examined. The tan 5 spectra of these composites show a second relaxation of relatively low intensity located about 40 degreesC above the main a relaxation, the glass transition T-g, which occurs at -34.5 degreesC in the unfilled polymer. This is attributed to an interfacial layer of polymer molecules whose chain relaxation dynamics have been altered by interaction with the filler surface. This is accompanied by a shift of the T-g itself to lower temperature when the filler surface is organophilic, but not when the filler surface is hydrophilic, and possible mechanisms for this are discussed. The amount of interfacial polymer can be quantified by resolving the glass transition and the second relaxation using a curve-fitting approach. A first-order treatment is presented which estimates the layer thickness to be of the order of a few nanometers. (C) 2003 Published by Elsevier Ltd.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available