Phthalate esters are used as plasticizer in many plastics, and several studies have shown their toxicity. Phthalate esters are gradually emitted over time, and so it is conceivable that they pose a significant health risk. This study aims to investigate the temperature dependence of the emissions of various phthalate esters and to estimate the health risks of these emissions at various temperatures. A passive-type sampler was developed to measure the flux of phthalate esters from the surface of plastic materials. With this sampler, we examined three widely used plastic materials: synthetic leather, wallpaper and vinyl flooring. The observed maximum emissions of diethyl phthalate, dibutyl phthalate, and diethylhexyl phthalate (DEHP) from these materials at 20degreesC were 0.89, 0.77, and 14 mug m(-2) h(-1), respectively. Emissions at 80degreesC were 2.8, 4.5 x 10(2), and 1.5 x 10(3) mug m(-2) h(-1), respectively. The results showed this temperature dependence is determined primarily by the type of phthalate ester and less so by the type of material. The estimation from the results of temperature dependence indicated the concentration of DEHP in a vehicle left out in the sunshine during the day can exceed the recommended levels of Japan Ministry of Health, Labour and Welfare. (C) 2003 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available