4.7 Article

Chemical degradation of fluoroelastomer in an alkaline environment

Journal

POLYMER DEGRADATION AND STABILITY
Volume 83, Issue 2, Pages 195-206

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/S0141-3910(03)00235-0

Keywords

chemical degradation; FKM (Viton A ); fluoroelastomer; XPS and ATR-FTIR; mechanical properties

Ask authors/readers for more resources

We have investigated the time-dependent chemical degradation of a fluoroelastomer, FKM (Viton((R)) A), in an alkaline environment (10% NaOH, 80 degreesC). Optical microscopy and SEM analysis reveal that degradation starts with surface roughness right from the earliest stage of exposure (e.g., 1 week) and finally results in cracks on the surface after prolonged exposure. Initially the extent of degradation is mainly confined to the surface regions (a few nanometers) but with longer exposure (e.g., 12 weeks) it extends to below the subsurface region of the fluoroelastomer. The extent of this surface degradation is found to be strong enough to affect the bulk mechanical properties. The molecular mechanisms of the surface chemical degradation were determined using surface analysis (XPS and ATR-FTIR) where the initial degradation was found to proceed via dehydrofluorination. This leads to double bond formation on the rubber backbone which accelerates the degradation even further with longer exposure. Furthermore, the cross-link sites of the exposed rubber samples are also found to be vulnerable to hydrolytic attack under the studied chemical environment as evidenced by the decrease in cross-link density and gel fraction (%). (C) 2003 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available