4.7 Article

Optimization of antireflection coating for VO2-based energy efficient window

Journal

SOLAR ENERGY MATERIALS AND SOLAR CELLS
Volume 83, Issue 1, Pages 29-37

Publisher

ELSEVIER
DOI: 10.1016/j.solmat.2004.02.014

Keywords

vanadium oxide; antireflection; luminous transmittance; thermochromism

Ask authors/readers for more resources

Vanadium dioxide (VO2) films have been proposed as energy efficient window coatings for their thermochromism, with which the solar energy transmission in the IR region may be controlled passively. These coatings suffer from low visible (or luminous) transmission (380-760nm in wavelength), which hinders their practical uses. We here consider an antireflection (AR) coating for the VO2-based window. Optical calculation was first performed upon a basic structure for thermochromic window composed of a VO2 layer on glass with an AR layer of refractive index n and thickness d. Optimization was carried out on n and d for a maximum integrated luminous transmittance (T-lum). The calculation demonstrates that the optimal n value changes with thickness of VO2, and at n approximate to 2.2 it gives the highest T-lum enhancement from 32% (without AR coating) to 55% for 50-nm VO2. Experiment was done on a structure of 50-nm VO2 on quartz glass using ZrO2, of which n,: 2.2 matching the best n value, as AR coating. Formation of an optimized structure, ZrO2 (56 nm)/VO2 (50 nm)/quartz, was done by sputtering, and its optical properties were characterized with spectrophotometry. An improvement of T-lum from 32.3% to 50.5% was confirmed for the semiconductor phase with similarity also for the metallic one. The IR switching properties were not much deteriorated. (C) 2004 Elsevier B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available