4.7 Article

Hot corrosion behaviour of a Ni plus CrAlYSiN composite coating in Na2SO4-25 wt.% NaCl melt

Journal

APPLIED SURFACE SCIENCE
Volume 268, Issue -, Pages 103-110

Publisher

ELSEVIER
DOI: 10.1016/j.apsusc.2012.12.012

Keywords

Superalloys; AlN; CrN; Composite coating; Hot corrosion

Funding

  1. National Key Basic Research Program of China, 973 Program [2012CB625102, 2010CB631206]

Ask authors/readers for more resources

Ni + CrAlYSiN nanocrystalline composite coatings and NiCrAlYSi reference coatings were prepared by vacuum arc evaporation on the Ni-based K438 superalloy. The aim of this work is to identify the hot corrosion resistance of the Ni + CrAlYSiN nanocrystalline composite coatings and the NiCrAlYSi coatings. The hot corrosion tests were carried out in a molten salt (75 wt.% Na2SO4 + 25 wt.% NaCl) environment at 900 degrees C. X-Ray diffraction (XRD), scanning electron microscopy (SEM) with energy dispersive X-ray spectrometer (EDX) and electron probe microanalysis (EPMA) technique were employed to characterize the coatings and the corrosion scales. The results indicated that both coatings improved the hot corrosion resistance of K438 in the molten salt environment. For the composite coating, the oxide scales were composed of alpha-Al2O3, Cr2O3 and minor NiCr2O4. No spallation or crack of the oxide scales was observed. Internal oxidation was detected in the outer part of the coating after 100 h corrosion. Internal TiN and AlN formation in the substrate was detected. In contrast, obvious crack/spallation of alpha-Al2O3 oxide scales on the NiCrAlYSi coating was observed; internal oxidation and sulphidation in the coating and even in the substrate were detected. (C) 2012 Elsevier B. V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.7
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available