TiO2 thin films with high dielectric constants (83-100) were grown on a Ru electrode at a growth temperature of 250 degreesC using the atomic-layer deposition method. The as-deposited films were crystallized with rutile structure. Adoption of O-3 with a very high concentration (400 g/m(3)) was crucial for obtaining the rutile phase and the high dielectric constant. The leakage current density of a TiO2 film with an equivalent oxide thickness of 1.0-1.5 nm was 10(-6)-10(-8) A/cm(2) at +/-1 V. All these electrical properties were obtained after limited postannealing where the annealing temperature was <500 degreesC, which is crucial to the structural stability of the Ru electrode. Therefore, these TiO2 films are very promising as the capacitor dielectrics of dynamic random access memories. TiO2 films grown on a bare Si wafer or Pt electrode by the same process had anatase structure and a dielectric constant of similar to40. (C) 2004 American Institute of Physics.
Authors
I am an author on this paper
Click your name to claim this paper and add it to your profile.
Reviews
Recommended
No Data Available