The effect of oxidation time and storage conditions on the surface wettability of thin films of polydimethylsiloxane (PDMS) spun cast onto glass slides was studied. Films were oxidized in a low temperature air plasma for either 1 min or 6 s and stored in either air, water, or hexadecane. Analysis of the sessile water contact angle with time shows that partial to complete hydrophobic recovery occurs within days under all conditions. (C) 2004 Elsevier B.V. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.6
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available