Glazed tiles manufactured from incinerated sewage sludge ash and clay

Journal

JOURNAL OF THE AIR & WASTE MANAGEMENT ASSOCIATION
Volume 55, Issue 2, Pages 163-172

Publisher

AIR & WASTE MANAGEMENT ASSOC
DOI: 10.1080/10473289.2005.10464614

Keywords

-

Ask authors/readers for more resources

Sewage sludge incineration is applied extensively in highly populated cities as a final sludge treatment. In this study, incinerated ash was utilized as an additive to clay to manufacture glaze tiles. Four different amounts of ash (0, 15, 30, and 45%) were added, and five glaze concentrations (0.03, 0.06, 0.1, 0.15, and 0.2 g/cm(2)) were applied on the surface of biscuit tiles to study the effects of ash additive and glaze concentration on properties of fired samples. Sewage sludge was dehydrated and incinerated into ash at 800 degreesC. Subsequently, tile specimens were manufactured and fired at 800 degreesC to make biscuit tiles. Fritted glazes and iron oxide were used as the fundamental glaze and colorant, respectively. Finally, glaze was applied on the surface of biscuit tiles and then fired at 1050 degreesC to sinter them into glazed tile specimens. Tests were performed to analyze properties, including water absorption, firing shrinkage, weight loss on ignition, abrasion resistance, bending resistance, acid-Alkali resistance, and aging resistance on specimens of glaze tile. To further understand more about the microstructural behavior of glazed tile specimens, analysis of energy dispersive spectrometer, scanning electron microscopy, and X-ray were carried out in this study.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.1
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available