Enzymatic degradation of PLLA-PEOz-PLLA triblock copolymers

Journal

BIOMATERIALS
Volume 26, Issue 16, Pages 2803-2811

Publisher

ELSEVIER SCI LTD
DOI: 10.1016/j.biomaterials.2004.07.064

Keywords

PLLA-PEOz-PLLA; proteinase k; biodegradable; enzymatic degradation

Ask authors/readers for more resources

The enzymatic degradation of poly(L-lactide)-block- poly(2-ethyl-2-oxazoline)-block-poly(L-lactide) triblock copolymer (PLLA-PEOz-PLLA) was investigated using efficient enzyme proteinase K. PLLA-PEOz-PLLA solution-cast film lost a considerable amount of hydrophilic copolymers in the first 2 h, and the degradation after 2 h proceeded predominantly by surface erosion. The two faces of the hydrolyzed film exhibited different morphologies following enzymatic degradation. The lower face showed many spherulites, which are the superstructural morphology of polymer crystals. Porous spheres based on crystalline PLLA were observed on the upper face, because they were more resistant to enzymatic attack. The crystallinity of the films increased monotonously with the hydrolysis time, thus, the absorption of water gradually decreased. The analysis of degradation residues revealed that many colloids of poly(2-ethyl-2-oxazoline)-co-polyethylenimine (PEOz-co-PEI) copolymers were dispersed in the buffer solution. The average diameter, 1 mum, of the colloids was reduced to 200 nm by advanced degradation. The proteinase K exhibited remarkable hydrolysis not only at the ester bond but also the amide bond. (C) 2004 Elsevier Ltd. All rights reserved.

Authors

I am an author on this paper
Click your name to claim this paper and add it to your profile.

Reviews

Primary Rating

4.8
Not enough ratings

Secondary Ratings

Novelty
-
Significance
-
Scientific rigor
-
Rate this paper

Recommended

No Data Available
No Data Available